Resource Center

FAQs

Permacorr can only be used on new carbon steel or on existing steel as a maintenance coating. It must not be used on galvanized surfaces, electroplate, or anywhere that residual zinc metal has been used. For additional specifications, see our technical data sheets (TDS) Permacorr Technical Data Sheet and Permacorr Gun Cleaner Technical Data Sheet.

Permacorr is a very fast reacting, two-component coating that requires a 1:1 ratio plural spray pump with 30:1 ratio (or greater) for application. For specifications see our Permacorr Application Guide. Watch a 35-second video of Permacorr being applied to a flash-rusted steel tank.

Only one coat is required. We recommend intermittent inspection and repairs depending on levels of corrosivity. For details see our Permacorr Application Guide.

Yes! Permacorr offers a breakthrough solution for CUI prevention. Unlike standard anti-corrosion coatings, Permacorr forms a true chemical bond with steel at the molecular level. It has been tested and engineered for ambient to high-temperature service up to 250°C (498°F).

For more details and to request a white paper on the use of Permacorr to prevent Corrosion Under Insulation, visit our CUI page .

Permacorr does not require a topcoat, but it is recommended especially for UV and dirt protection. If a topcoat is desired, only topcoats approved by Advanced Polymerics Inc. should be used.

Permacorr is a water-based protective coating that has no VOCs, virtually no odor, contains no biocides and uses food grade ingredients. It is non-flammable and non-combustible so can be stored without special precautions. To see its other safety benefits, please view the following:

No, Permacorr is for external use only on carbon steel.

Yes. Permacorr will tolerate flash rusting, since it reacts with rust in a similar way to its reaction with steel. It can even tolerate rain droplets soon after application. For details see the Permacorr Application Guide.

In less than 5 minutes, Permacorr will be dry to touch. Permacorr needs a few hours to harden, and this depends on temperature as well as humidity. As a guide, Permacorr can tolerate rain within 30 minutes of application.

Permacorr is engineered to extend asset life while reducing total lifecycle costs through faster application and long-term performance. Corrosion is a leading driver of increased maintenance costs, unplanned downtime, and premature asset replacement across tanks, piping, and infrastructure. 

Watch the recorded webinar (~ 47-minute event hosted by Storage Terminals Magazine) to learn what corrosion truly costs, how coatings work to prevent or reverse rust, and review case histories showing how others are using Permacorr to combat corrosion and extend asset life.

Permacorr can only be used on new carbon steel or on existing steel as a maintenance coating (seek guidance for specialty steel alloys). It must not be used on galvanized surfaces, electroplated surfaces, or anywhere residual zinc metal has previously been used. For additional specifications, see our technical data sheets (TDS): Permacorr Technical Data Sheet. 

Permacorr is unlike any other coating on the market. It chemically bonds to steel, unlike epoxy coatings which are rolled onto steel and adhere to the metal surface. Permacorr’s chemical bond creates a permanent layer between the metal and the coating. When moisture penetrates epoxy, it creates a bubble by osmosis allowing corrosion to start between the steel and the coating.

This time-lapse video (1 minute long) illustrates how quickly steel corrodes when uncoated or when coated with epoxy compared to Permacorrr. 

Permacorr is truly unique in that it not only prevents but also reverses corrosion

  • The Permacorr-coated panel is on the right 
  • You can see all panels are “scribed” to the substrate 
  • If you look closely, rust begins to form on all panels, but on the Permacorr-coated panel, the rust in the scribe disappears
  • Permacorr is truly unique in that it not only prevents but also reverses corrosion

Unlike other anti-corrosion treatments, Permacorr contains no low-molecular-weight epoxy resin. Therefore, it will not cause an allergic reaction resulting from repeated skin exposure to uncured epoxy resin or hardeners, which can lead to dermatitis, rashes, itching, and swelling. Nevertheless, skin and respiratory protection should be used in close proximity to spray operations. Good hygiene standards are always recommended.

No, Permacorr is for external atmospheric use only—and can only be used on carbon steel.

Yes, Permacorr is more than just sustainable. It is designed to be longer-lasting and can self-repair minor damage between maintenance intervals.

It also has a very low CO2e value of 2.22g per micron/m2 and has no solvent emissions, no VOCs, and has very low toxicity compared to alternative anti-corrosion coatings.

Yes, Permacorr has been used on large-scale tanks in refineries and storage terminals, contact us for further details.

Fire Water Storage Tanks with Permacorr and topcoat.